looking nice. i used to make orgonite for over 8 years, did a lot of gifting. works great. just a friendly advice, you need more metal in there, best is 50metal/ 50 resin ratio. with too little metal in the orgonite it would output too much DOR instead o wanted POR...
03:28 PM - Apr 09, 2021
In response Carminda Camara to her Publication
Only people mentioned by prdka_la_bleu in this post can reply
Carminda Camara
@CarmindaC
09 April, 04:31
In response milanek holograph to his Publication
i put it at the base ... under my symbol ... i’ve used Copper under it